CNC machining, plastics first
CNC machining for plastic. Tolerances stated by material.
Plastic is not soft aluminum. It grows with heat, relaxes after the cut and smears under a dull tool. Upload a part and the price comes with a manufacturability check whose wall, corner and hole rules are set for plastic, not borrowed from metal.

What each plastic will hold here
| Material | Standard | Tightest quoted | What moves it |
|---|---|---|---|
| Acetal / Delrin | ±0.005" | ±0.002" on a called-out feature | Little. The plastic to pick when a dimension matters. |
| UHMW | ±0.010" | Ask | Temperature, and it springs away from the cutter. |
| HDPE | ±0.010" | Ask | Temperature. About ten times the expansion of steel. |
Plastic expands five to ten times as much as steel for the same temperature change, so tell us where the part lives. A plastic not listed here is quoted with its tolerance stated before you order.
What belongs on a mill
- Blocks, brackets, clamps, saddles, wear pads and guides in acetal, UHMW and nylon.
- Housings and manifolds in acetal, polycarbonate, PVC and polypropylene.
- PEEK and Ultem for heat, chemical or electrical duty. G-10 and phenolic when the part has to be stiff and insulating.
- 6061 and brass are priced online too, for the part that mates with your plastic one.
Machines and limits
- 4th-axis indexing for parts with work on more than one face.
- The instant quote takes milled parts up to 18" × 9.5" × 12" (457 × 241 × 300 mm). Anything larger is quoted by a person.
- Round work: a manual lathe, to 10" diameter × 36" long, for tight-tolerance bores and second operations on parts run on the other machines.
- Up to 100 pieces prices and checks out online. Over 100, a part the check fails, or a line over $5,000 goes to a person first.
Design notes that save you money
- Inside corners carry a tool radius. The check asks for a radius of at least one third of the pocket depth, and the smallest cutter it allows is 1/16".
- Walls: 0.060" (1.5 mm) or more in most plastics. Under 0.040" (1.0 mm) gets flagged. Acrylic, G-10 and phenolic want 0.080" (2.0 mm).
- Pockets deeper than four times their width and holes deeper than four diameters cost more, and the check says so.
- Put the tight number only on the feature that needs it. That is where most of the price of a plastic part comes from.
- If the part is really a flat profile under 1" thick, routing usually costs less. Switch the process in the quote tool and the price changes on the screen.
What gets sent elsewhere
Better you hear it here than after you have waited for a quote.
- Square inside corners. Those are a broach or an EDM job, which this shop does not do.
- Heavy aluminum production. A metal shop will serve you better.
- A tolerance the material will not hold. Plastic expands five to ten times as much as steel for the same temperature change, so tell us where the part lives.
- Finishes: Anodize and powder coat are sent out to a finisher. Bead blasting is done here. A part with a sent-out finish ships on the standard lead time.
Materials priced online
Full material guide →Delrin / acetalUHMWHDPENylon 6/6 & castPEEKUltem (PEI)PTFEPolycarbonateAcrylicPVCPolypropyleneG-10 / FR-4Phenolic6061-T6Brass 360